s is the fact that of the substrate material. The lattice mismatch causes a significant buildup of pressure Power in Ge levels epitaxially developed on Si. This strain Electricity is primarily relieved by two mechanisms: (i) generation of lattice dislocations on the interface (misfit dislocations) and (ii) elastic deformation of each the substrate